differential scanning calorimetry instrumentation available

Netzsch Instruments
Maia DSC 200 F3

DSC 200 F3 MaiaNetzsch Instruments

Features:
  • Thermal characterization of solids and liquids
  • By applying a controlled temperature program (isothermal, heating or cooling at constant rates), phase changes can be characterized and/or the specific heat of a material can be determined.
  • Values such as the Onset Temperature, Peak Temperature, Peak Area (i.e. Enthalpy) and/or Glass Transition Temperature (Tg) can be obtained from the resulting curve
  • Atmosphere: Nitrogen
  • Temperature Range: -40 to 600°C
  • Max Heating Rate: 100K/min
  • Temperature Profiles: Isothermal, Heating and Cooling at controlled rates
Applications:
  • Melting/crystallization behavior
  • Decomposition behavior
  • Purity determination
  • Specific heat
  • Call for additional specific applications
Recommendations for Optimal Output:
  • Sample Weight: 2-50mg optimal (if sample quantity is an concern, please call to discuss)